Hi Guys,
I'm new here, but have found this particlar thread to be incredibly helpful in building a battery spot welder. I'll try to post some pictures soon.
Main welding power source is a 12V 710CCA car battery.
Used ten IRF3205 mosfets on a 1"x1/4" aluminium flat bar.