Hello, I need someone who can help me please
I bought SAMSUNG 35E cells to rebuild my DERBY CYCLE 36V 13Ah battery, because I had little time to work.
After having done all the work, the battery does not work. and I do not know why.
The battery does not have voltage across the BMS, but if...