Here is the best shot I have of the bottom of the battery flipped upside down. I could get some access but seem stuck on how to remove those wire connectors. I see no release mechanism. Do you. If I have to pull those individually and they come off of the low voltage batteries. Do I create a...
I forgot to mention, I have tried opening it from the bottom and I am either dumb as a fence post or This has some kind of real trick to opening. Probably for some really good reasons. Do you know how this thing should ope. Hoping I wont splash some kind of acid on me by trying. Here is the...
Here are the specs of the battery image lower right.
Lookn down into the cavity of the top of the battery and it appears there are 8 of the packs inside each Cell. There are a total of 9 30 V batteries for a total of 270 Volts.
I read LG Chem , Tyco Electronics & PA66-TD30 or maybe TO30...
When you say get into the cells itself. We opened the battery casing and individually extracted the cells 9 of them 30 v each or 270.
Or are you referring to 4 going in and charging the 4 square aluminium encased parts inside the 30 v seen below.
Thank you so much for this help. Any and...
I have a Hyundai /Kia Sonata Hybrid Battery. The cells are 30 volt Lithium
I purchased a Grin Technologies Satiator Battery Charger Standard 12v to 52v