Hi all,
I purchased a number of items from em3ev a while back. I have only recently finished my e-motorcycle build and taken it for a few test runs. It was my first taste of electric vehicle power! Very exciting! However, I have quickly run into a multitude of issues with the MQCON/Sabvoton...
Hi all,
I'm having trouble with my Sabvaton 7280 controller. It's showing Error 02H on the LCD, which (as far as I can tell) is an "over voltage" error. Perhaps it is linked with the fact that when I connect the MQCON app, it shows battery voltage as being 92V. However, this is not the correct...
Hi all,
I've recently completed a conversion of an old Honda XL185. Unfortunately I've just found out that some of the battery wiring is beginning to degrade quite seriously.
I was worried from the start about the wire I was using, it feels very "flimsy": I thought maybe this was because it...