Hi
Opened my fake battery for Makita tools.
Stated capacity is real, 6Ah (5s3p, 2Ah cells), tested with icharger (6.3 Ah)
Max discharge rate the charger can do is 7A, took 40 min to take the voltage down to 15v, and cells were mildly warm.
But apart from that, cant find anything about these...