Old thread.. but looks like no freewheel so regen possible, would be nice to see if this project was ever finished some nice machine work going on there... with a good battery no doubt this thing would be an animal.
Just add support legs that extend forward then you need zero counter balance like the walk behind lifts...
Otherwise lift less or add some weight, concrete as suggested above would be most cost effective and coming close to the weight. Most battery's are 2k-3500lbs in those lifts (its stamped on...
bigger outrunner (8057) just considering options for better start up power, other wise the edge160 works.
phaserunner looks interesting but lower amps definitely a possibly just to try the sensored performance out.
What kind of options are there for a 12s lipo compatible brushless sensored esc(ideally 100amp or more).
Basically a sensored version of the castle edge hv160 is what im looking for.
Trying to avoid cheap china controllers if possible...
if you put them in series the ah and amp draw rating stays the same , parrallel would make them addup.
that battery is rated for 40A 40ax36v=1440w you can run that motor just dont expect to see 5kw.
2 in series 2.8kw
thanks for the input that's currently plan b, and it can be done a bit cheaper with some of there other battery's. I'd like to know if any other ev car battery's will work cheaper. so far the ford e max cells look like they might work. most of the others seem to large to have 24s in a bike or...
looking for some options/opinions on a battery for use in a future motorcycle project. peak power should be around 40kw assuming 24s(100v) 400a. obviously weight/space is somewhat critical, don't have a capacity in mind but aiming for 5kwh roughly (50mile range?). have been looking at various ev...
most of the power supply's (unless they are c.c) will do that. they think its a dead short and will go in to fault or protection mode. "Protection type : Hiccup mode, recovers automatically after fault condition is removed" you can use a current limiting board inline with the power supply to...