  1. H

    spot welder recommendation: Glitter vs Sunkko for .3mm pure

    Hello all. I am planning to start a new battery build, and I was interested in buying an off the shelf spot welder that could do .3mm pure nickel. Though I am open to kits as well. At the moment, I was considering the Glitter 801D or the Sunkko 709. Any thoughts? I couldn't find much on this...