Just did a test tigging of a couple of pieces of tube. Semi-destructive testing shows it to be plenty strong, and penetration was OK, but I did get a bit of burn-through and warping, and it's a bit bodgy looking, I was wondering if anyone had some advice on technique (apart from not rushing...