Hello all,
I recently put together a 24S2P (72V, 20Ah) LiFePo4 pack made up of 10Ah Headway cells for an e-bike project. It is connected to a BMS that has performed flawlessly in the past.
After the pack (about 50% charged) was installed into the bike, the bike worked great. Then I charged it...