  1. S

    Anyone have any tips on rewinding MXUS 3k?

    There are a couple of hub motors around here that have been run too hot and then left to stand resulting in blackening of the windings in one particular area. One is an MXUS 3k and another is a similar clone. Needless to say they don't work any more due to current leakage between the wires...
  2. S

    A minimal Q76 offroad build

    Frame: Q76 Forks: Rockshox Boxxer RC Shock: Rockshox Vivid Brakes: Shimano Saint Cranks: Raceface Chester Bars & Stem: Raceface direct mount 35mm Rear wheel: 19" Holmes MMP rim & Shinko trials tyre Front wheel: 24" Halo SAS & Vuelta 24x3" tyre Motor: Cromotor V2 18x4 winding 9.7kV Controller...
  3. S

    Adaptto Max-E Fault

    Hey everyone, My Max-E stopped working suddenly during a charge. The symptoms are: When charging the PSU is shorting and going into overheat protect mode whilst "no charge voltage" is displayed on the computer. When trying to run the motor it just rocks back & forth. So I see no errors on...
  4. S

    Looking for fluent English speaker w/ a fast off-road enduro

    I have been into two wheeled things for years and have a garage full of cycles and motorbikes, but until the weekend I had never seen an electric enduro bike, and now I can't get the idea out of my head. My main passion is offroad MTB enduro riding, so one of these would be great for adventure...