• Howdy! we're looking for donations to finish custom knowledgebase software for this forum. Please see our Funding drive thread

Search results

  1. B

    Mac motor parts needed

    What's the size of those cover plate screws?
  2. B

    Electric Buell racebike build

    Not my build, but here are a few sources: http://thunderstruck-ev.com/me1507.html https://www.emf-power.com/product/motenergy-me1507/ https://www.electricmotorsport.com/ev-parts/motor-drive-kits/brush-less-pmac-motor-kits
  3. B

    Electric Buell racebike build

    Hi Stamen, Checking in to see if there has been any progress on your build....hope all is well.
  4. B

    E-Ducati Build

    From my understanding they are the exact same motor minus some minor tweaks in performance between Me1507 and 75-7. 75-5 is thinner.
  5. B

    E-Ducati Build

    I have been working on some more models/CAD files: https://grabcad.com/aastan.gadson-1
  6. B

    E-Ducati Build

    Link repaired
  7. B

    E-Ducati Build

    Hi, I just subscribed. I am planning a similar build as I am graduating from e-bikes :D (check my signature). I posted a CAD file of the ME1507 motor recently as I couldn't find one to mock up my bike in Fusion360. I placed a link to it below if it may be of some help to you. I have not...
  8. B

    Custom eBike Based on Enduro Frame

    See video for details of build. Throttle is from Paul at EM3ev. Not sure the model exactly, but he matched it to the controller I also purchased from him.
  9. B

    Custom eBike Based on Enduro Frame

    The frame has held up well. Only flat riding here in the South (SC). I have discovered a little rust developing on the swing arm near the axel. This just means they need a better painting and treating method. I made a few mistake with parts seen in my latest videos. The original list is...
  10. B

    What fuse to use?

    T-Spec available from 100-200amp http://www.ebay.com/itm/T-Spec-V12-CBF100-Gold-Plated-Circuit-Breaker-100-Amp-1-0-Or-4-Awg-In-Out-New-/131727168728?hash=item1eab8d14d8:g:E3cAAOSwzgRWv3lU&vxp=mtr
  11. B

    Custom eBike Based on Enduro Frame

    -hcGNDh0G0k
  12. B

    My New Build Bomber Style 100V 26Ah 8kw MC Rims and Tires

    Great build! What size are the 244's?
  13. B

    Custom eBike Based on Enduro Frame

    4w5LfkYvpyA
  14. B

    Custom eBike Based on Enduro Frame

    Batteries in and tested. A total of 200 Sanyo 18650GA 3.5ah. They all arrived at 3.50v and the capacities look good!
  15. B

    Custom eBike Based on Enduro Frame

    Everything fit perfectly. Only short coming is the pack of used cells. Only able to deliver 2amps per cell which is 20amp peak accounting for resistance and age. Building new pack of Sanyo 3.5ah 10amp 18650GA cells. That's 100amp peak (20s10p). Suspension is good tires are great for the...
  16. B

    Custom eBike Based on Enduro Frame

    First ride after battery pack completed. Enduro frame 72v with 20ah 18650 pack.
  17. B

    Custom eBike Based on Enduro Frame

    Here they are painted black with new 12V led lights added.
  18. B

    Custom eBike Based on Enduro Frame

    My standard 8.4v headlights before modification.
  19. B

    Custom eBike Based on Enduro Frame

    Not of the current BMS because it was defective. Went through two cycles of charge and dis-charge and on the third time charging to full capacity the BMS stopped working. The balance light indicators won't light up anymore. New BMS should be here by Friday and I will go through the testing...
  20. B

    Custom eBike Based on Enduro Frame

    This will be the last photos for this pack. I ran into a setback when I shorted the BMS the new one should be here by the end of the week. A new full 72V pack was purchase just incase I run into more issues. If not, the new pack will be put on my second build. One last video will follow as...
  21. B

    Custom eBike Based on Enduro Frame

    Hi Lurkin, I am glad you like the videos. This is my first build and I, like so many others, have used a lot of resources here on ES and Youtube. I found Damian Rene here: https://www.youtube.com/channel/UCPYVGWdT858wIc1LEeB1o7A and actually took his recommendation for the BMS from his...
  22. B

    Custom eBike Based on Enduro Frame

    Here is the latest video. The pack completion will be broken up into 2-3 videos: QCci5puqkWY
  23. B

    Custom eBike Based on Enduro Frame

    Battery as it stands today. I will be making small changes, video coming soon.
  24. B

    ENDUROEBIKE.COM

    Hi Quadfather, I want to share my new build with you. What size change (500 or 700, etc.). I have that same tensioner, any pointers you can point out to me would be greatly appreciated. Link: https://www.youtube.com/user/adminaeg/videos?view=0&sort=da&flow=grid
  25. B

    Custom eBike Based on Enduro Frame

    The pack is welded. Picked up a 220V welder off of eBay. I have received good results from it. Tabs are cut from .8 x .15 nickel strips. Video coming soon showing details of the pack to include soldering poser leads, BMS soldering, and how it is covered.
Back
Top