    Battery Flyer 36V Panasonic BMS problem: won't charge

    Battery Flyer 36V Panasonic BMS problem Hello, the battery was 4 years old and the cells were exhausted, and I decided to buy 40 cells Samsung 29E and change them, after finishing the work I check the voltage of the cell pack and it is 35.7 V I connect the BMS and the lights are on sequentially...
  2. R

    Battery rebuild derby cycle 36v 13Ah

    Hello, I need someone who can help me please I bought SAMSUNG 35E cells to rebuild my DERBY CYCLE 36V 13Ah battery, because I had little time to work. After having done all the work, the battery does not work. and I do not know why. The battery does not have voltage across the BMS, but if...