Hello,
I am building huge 12S14P battery pack. To do this i have got access to professional spot welder in academic laboratory with ADP3 weld power supply (300 Joule, dual pulse, stored energy welding power) and WBT-Q03 welding head.
I am using 0.2 mm thick and 7 mm wide pure nickel strips.