Hello everyone, I have been building my own Li-ion battery packs from past 6 months and was using 0.15mm thick nickel strip as my discharge current was hardly 17amps. But now I want to build a battery with 35amps discharging current so I had double spot welded my two nickel strips of 0.15 mm. So...