According to this http://www.diyelectriccar.com/forums/showthread.php?t=52468 thread, you can now buy the headway 40152S (15Ah cell).
Here is the specifications:
40152(3.2V15Ah) lithium battery cell, widely used for electric vehicles, with the long cycle life and wonderful function
Nominal...