I made a ebike a year ago and i changed hub motor because i broke aluminum disk in previous one and changed 3 controllers. I used a 36v battery max voltage 42v after 2 months i become greedy and added another 1s in 10s battery with other bms now i was using two batteries with 2 bms with 2...