Holy smokes man just look at you.
Note that I'm not surprised they don't add much 45/45 weave in those tubes, because if they're in a truss-type situation, then the tube elements are back into axial loads, and not torsion, so 90/0 is all they need. So you're kind'of a special case, and I think...