Trying using your esp32 code here to set to 42V, works like charm. But when I turn off the esp32, in about 40 seconds, the r48-3000e3 revert back to 51.8V (no load, just test using voltmeter). The set voltage offline should set the default voltage permanently right? So I can't use relay because...