i am trying to make a spot welder using a 12v 300 cold crank amps battery with a 12v cylinoid with a switch im using 10gage leads to copper roofing nail tips. the welder isnt getting a good contact for welds for some reason. whether i do a quick burst or hold it there for abit and get it red in...