opperpanter
100 W
Couldn't find any topic on this cell, so here's one
Samsung INR1865035E
Some curves: http://www.dampfakkus.de/akkutest.php?id=577
capacity 3500mAh
Minimum Capacity 3350mAh
Voltage 3.6V - 3.7V
Charge voltage 4.2V
Discharge current ( constant ) 2,5C 8A
max . Discharge current ( constant ) 3C 10,5A
Charging current 0.6C 2000mA
discharge voltage 2,65V
Protection circuit PCB No
Positive flat ( FlatTop )
Chemistry LiNiCoAlO2
Diameter 18,55mm ± 0.1
Height 65,25mm ± 0.15
Weight 48g ± 1
CC-CV charging method
If it really gives 3450mAh, it's a great improvement over the 29E at the same weight.
[moderator edit to change title after thread subject expanded]
Samsung INR1865035E
Some curves: http://www.dampfakkus.de/akkutest.php?id=577
capacity 3500mAh
Minimum Capacity 3350mAh
Voltage 3.6V - 3.7V
Charge voltage 4.2V
Discharge current ( constant ) 2,5C 8A
max . Discharge current ( constant ) 3C 10,5A
Charging current 0.6C 2000mA
discharge voltage 2,65V
Protection circuit PCB No
Positive flat ( FlatTop )
Chemistry LiNiCoAlO2
Diameter 18,55mm ± 0.1
Height 65,25mm ± 0.15
Weight 48g ± 1
CC-CV charging method
If it really gives 3450mAh, it's a great improvement over the 29E at the same weight.
[moderator edit to change title after thread subject expanded]