given the same bike setup e.g.mtb,26"wheels,hs3540 motor and lyen 36,40amp controller...is there a range difference between an a123 lifepo4 36v,20amp battery and a 36v,20amp lipo battery....and of course, same speed[25mph] and terrain
kriskros said:given the same bike setup e.g.mtb,26"wheels,hs3540 motor and lyen 36,40amp controller...is there a range difference between an a123 lifepo4 36v,20amp battery and a 36v,20amp lipo battery....and of course, same speed[25mph] and terrain
my pack is 108 cells built by cell man..nominal voltage 39.8.... therefore,having a tadpole trike, the a123 battery ius better for me,especially considering the great difference in life... on a trike size and weight are not a problem... thanks allSamTexas said:Yes, there will be a small to negligible difference in range.
A123: Nominal voltage is 3.3V. 11 cells are needed to make a 36V battery. Actual nomimal voltage is 36.3V, actual capacity is 726Wh.
RC Lipo: 3.8V, 10 cells, 38.0V, 760Wh.
So in theory the 36V RC Lipo will give you 4.7% more range.
ive never seen a supplier list a 36v,battery as 39.3or anything else other than 36volt.. since i am considering another build, i really was curious toknow if there is range difference between lipo and lifepo4 batteries of the same voltage and amperage..life expectancy i am aware of... sorry if i disturbed your equanimitySamTexas said:You are not welcome. Why did you ask in the first place?
Your question was SPECIFICALLY about:
1) 36V battery, either A123 or Lipo: There's no such thing as a 36V battery for those. The closest is 11 cells for A123 (36.3V) and 10 cells for Lipo (38.0V). Now you came back and say a 12 cell A123 battery is better. Of course it's better because it's NOT a 36V battery. You could have bought a 20 cell (66.0V) A123 battery and call it 36V if you want too.
2) which gives you a better range. No where did you mention life expectancy in your question, but now it's one of your deciding factor.
I don't give a hoot about which battery you end up with, I was just trying to answer your damn question.
hnasc said:kriskros said:given the same bike setup e.g.mtb,26"wheels,hs3540 motor and lyen 36,40amp controller...is there a range difference between an a123 lifepo4 36v,20amp battery and a 36v,20amp lipo battery....and of course, same speed[25mph] and terrain
hi kriskros, what i want to say about bike battery The Suzuki make a good comparison as it has a top speed of 71.5 mph, vs. 68.1 mph for the Zero and a slightly quicker ¼ mile time of 18.37 seconds vs. 19.31 seconds for the Zero. However, the Suzuki has a slower 0-60 time of 13.62 seconds to the Zero’s 0-60 time of 11.73. The Zero makes a 22.58 hp on their dyno, while the Suzuki makes 13.29 hp, it has a 5-speed transmission and weighs slightly less, which evens the performance comparison. (That caught my eye. It would appear that having a transmission can compensate noticeably for a lower power motor.) The Suzuki weighs 276.5 pounds and the Zero weighs 296 pounds. The Suzuki got as much as 86.7 mpg in their testing and averaged 63.8 mpg in both on-road and off-road use. This gives the Suzuki a fuel cost of $0.069 per mile, compared with the Zero’s $0.03 per mile.
But then you have to compare maintenance. The Suzuki’s cost for filters, oil changes, valve adjustments, etc. would average an additional $0.062 per mile, compared with the Zero’s minimal maintenance requirements of cleaning and replacing its motor’s brushes at 8000 mile intervals and checking the bike over every 4000 miles. They estimate that this would add another $0.033 per mile to the Zero’s mileage cost.
However the big cost for owners of the Zero is the need to replace its $4000 battery, which, based upon their analysis would need to be replaced every 36,000 miles, assuming a range of 20 miles and a specified 1800 charging cycles. The price to replace the Zero’s custom-made battery choked them up quite a bit and that added another $0.111 per mile to the cost of ownership of the bike.
The grand totals come to a ownership cost (over 36,000 miles) of $0.174 per mile for the Zero DS and $0.131 per mile for the Suzuki DR200S. Note that this does not include the cost of insurance, tires, brake pads and other expenses shared by both motorcycles. Their calculations also don’t include the $10,495 price of the Zero, which is much more than the $4199 price of the Suzuki, although current Government incentives lower the final purchase price of the Zero. Naturally, the conclusion is that it is cheaper to purchase and ride the Suzuki, compared with the Zero at this stage in the technological game. But they conclude that if EV purchase prices drop, and performance and fuel prices increase, the economic cost to own IC and EV motorcycles will become more comparable, but right now the advantage is still with the gasoline-powered motorcycle.
If you have any question related to my this post so you can feel free ask to me...
hnasc said:kriskros said:given the same bike setup e.g.mtb,26"wheels,hs3540 motor and lyen 36,40amp controller...is there a range difference between an a123 lifepo4 36v,20amp battery and a 36v,20amp lipo battery....and of course, same speed[25mph] and terrain
hi kriskros, what i want to say about bike battery The Suzuki make a good comparison as it has a top speed of 71.5 mph, vs. 68.1 mph for the Zero and a slightly quicker ¼ mile time of 18.37 seconds vs. 19.31 seconds for the Zero. However,....
But then you have to compare maintenance. ..........
..... but right now the advantage is still with the gasoline-powered motorcycle.
If you have any question related to my this post so you can feel free ask to me...
AussieJester said:Out of curiosity Luke, legally what does 'life of the vehicle' mean in years? It
is surely hard to put a figure on how long the bike will last is it not? There are 30-40 year
old motorcycles being ridden around, would a battery be capable of lasting this long
with daily charging? I find this a lil hard to believe...? If it lasted 10-15 years with daily charging
and retained 85-90% capacity i would consider it pretty damn good and money well spent
... Just curious anywayz mate, not trying to be negative in anyway about the Zero its a damn
fine product
KiM
p.s no idea why hnasc posted this here but since he did thought i would ask haha
Joseph C. said:Is Luke not bound by a non-disclosure agreement about specifics? You don't want him to be sued, now do you Kim.
neptronix said:Yeah, 'life of the vehicle' is a pretty nebulous concept.. by some automakers, it is 100,000 miles.
I have not heard of a lithium battery that has a calendar life of more than 10 years. A brushless DC motor would theoretically last forever.. sooo..
Ive had my a123 battery since may/11 about 1800 miles and 90cycles..no problems. full charge always shows 43.3 volts...bms and battery suppliedby cellman.. voltage sag approx 39.9 to 38.6 after 18ah ride..CA reading ... and thats how i charge it..very happy999zip999 said:Kriskos how long have you had your a123 ? Are you happy with it ? What bms and has it had given you any problems ? Remeber you can plug your a123 and walk away and sleep at night. Alot less risk of FIRE.