hi guys,

i am louis raaijmakers and i am 16 years old and i live in the netherlands.
my english isn't so good i can speak it better than i write it. :)

i am goin to make my self a electric bike frame

1 or 2 weeks ago i bought 54 10 lifepo4 cells for a 72v 20 ah battery pack and 4 extra i bought it from electric...... he is frome france and it was within a week at my home.

so first i have bought a old canondale full suspention frame. when i put some forks and wheels in it it look terible.
so i am going to change it and make it diffrent.
i have found it online on a site called marktplaats.nl

yesterday i cut the headtube of the frame
also i removed the seatpost holder and the rear suspention of the bike.

today i have made the battery holder.

here is the site where is stole my idea's off :http://electrotransport.ru/ussr/index.php?topic=18196.0

now i am goin to see if i can put some photo's up.

thanks
 
here are some photo's

fist the box where the battey's came in
https://www.flickr.com/photos/123475183@N04/13901354293/

the frame wat is was goin to use first.
https://www.flickr.com/photos/123475183@N04/13901346213/in/photostream/

the battery weight.
https://www.flickr.com/photos/123475183@N04/13901276395/in/photostream/
 
again some photo's

the first frame for the bike.
https://www.flickr.com/photos/123475183@N04/13916691631/in/photostream/

drawing
https://www.flickr.com/photos/123475183@N04/13916682331/in/photostream/

second fame done now i need some new second hand forks +- 200mm travel.
and maybe i am goin to change the rear suspention. :)

but you will hear it.

and any options for making the bike better an welcome so please coment.
bye bye
 
today i went on after my internship.
i first was figuring out how i would build the bike.
this are my foto's where is stole my idea's of:
http://imageshack.com/a/img843/2127/dzqb.jpg

then how do i want the suspention? 3 options.
1 http://imageshack.com/a/img843/1206/d8l1.jpg
it looks ugly....not a option.

2 http://imageshack.com/a/img841/2101/t8ze.jpg
doesn't look so bad at al. this rear suspention bridge i took of a honda ns1 frame.

3 http://imageshack.com/a/img842/5886/uhw9.jpg

make my own suspention and use the parts from the 1 picture.


and here some picture's from my intership. by Heavac.
right now we are working in belgium. for the bus making company van Hool.
maybe i also go with them to france and norway.

the also have hydrogen busses and the have 2 battery packs of 120s 2 pack :shock:

http://imageshack.com/a/img838/9908/llxb.jpg
http://imageshack.com/a/img842/2798/v2ht.jpg
http://imageshack.com/a/img834/8738/vndi.jpg
http://imageshack.com/a/img843/5537/ye97s.jpg


greeting louis
 
Hi,
I'm building a frame that looks similar to yours: http://s1.directupload.net/images/140402/twhb9mnm.jpg
I made my own swingarm. The swingarm of my downhillbike did not allow the suspension to be outside the frame.
Check out this thread: http://endless-sphere.com/forums/viewtopic.php?f=6&t=29555#p426619
 
hi nice to see.
i am goin to make the frame today ready.
but do you also have a tread?
i would like to follow you update's
and where dit you get you front fork off?

and if anyone know how i can get the so that they show up directly on the site i would appraciate that.

sorry for my bad english

greeting louis
 
I have a thread that I haven't updated for a long time: http://endless-sphere.com/forums/viewtopic.php?f=6&t=53234
As soon as I have the bike finished, I will post pictures etc...
The fork comes from a downhill bike I bought for 600€. I am using several parts of it, as they are rigid and suitable for the heavy bike that I'm going to build.
There are some threads that I took ideas from:
http://endless-sphere.com/forums/viewtopic.php?f=6&t=50575
http://endless-sphere.com/forums/viewtopic.php?f=6&t=34880&hilit=farfle+THIS+year&start=50
http://endless-sphere.com/forums/viewtopic.php?t=38667
http://endless-sphere.com/forums/viewtopic.php?f=6&t=23143&hilit=custom+frame
You can insert pictures directly by clicking on the Img buttom above the text field.
 
hi some new photo's

looking good and the build is still going "fast".

louis
enjoy

some idea's of the suspention. spotwelded and when i put it on the ground it calapst :p

http://imageshack.com/a/img841/9347/34a0.jpg
http://imageshack.com/a/img838/6543/v8sf.jpg
http://imageshack.com/a/img834/9802/543q2.jpg

more to come
 
louis raaijmakers said:
and if anyone know how i can get the so that they show up directly on the site i would appraciate that.
http://www.endless-sphere.com/forums/viewtopic.php?f=13&t=14748
 
I'm not a frame builder and only have a little welding experience, but I would take that collapse from it's own weight as a sign. I think the piece holding the TOP of your rear shock should be as short as possible without making the shock touch the frame as the suspension compresses, and add a gusset to the top of that support above, attaching to and running along the part of the main frame going to the seat tube support.

What is the wall thickness of the tubing you are using? With such a small size of tubing, I would be afraid of not having enough surface area for the welds to be strong enough, and a larger size of tubing can have a much thinner wall and be stronger than a smaller size with thicker walls.

I like your design and the amount of space you will have for batteries, but I think you will need a lot of bracing with such small square tubing.
 
hi,
sorry you are mis understanding.
i was done with the bike for that day and just weded it for 3 seconds and only on the rear side.
also the top mount of the rear suspention is goin to be a triangle and not a single tube as it is now.

trust me the bike is goin to be strong! (also heavy :oops: )

i wil work the whole day on it tomorow if i can get out of my bed... (party :) )

thanks for the good words
 
Consider moving shock attachment to between swingarms or the bottom of swingarm. Then frame end attachment point can move to stronger part of the frame and more forward for a more linear compression stroke. Stronger and lighter. I think it will look much cleaner too. Many modern motos do it that way. My computer is all screwed up and even Paint doesn't work or I would draw what I mean.
 
ebike met achter veering china.jpgView attachment 2hi,
today i have been thinking alot and also have made some change's on the bike.
first i wanted to fix the rear suspention.
so i got my dad involved with this. becouse i first wanted the honda rear suspention on the bike.
but my opinion was it wasn't at the angle i wanted....
he said it was probely to stiff i also thought about this but i just wanted to try it the he said.
why not use a shorter spring so you can place it easer under the box.
so we came to the idea of ussing the old suspention. and up greading it later.
here are som pic's



more text tomorrow.
 

Attachments

  • IMG_20140503_174631[1] (600 x 450).jpg
    IMG_20140503_174631[1] (600 x 450).jpg
    53.6 KB · Views: 8,904
  • IMG_20140503_174703[1] (450 x 600).jpg
    IMG_20140503_174703[1] (450 x 600).jpg
    55.3 KB · Views: 8,904
i also made my own rear suspention "bolt"
parts picture and result :)

and also a gangster picture of my self as a welder :roll:
 

Attachments

  • IMG_20140503_174455[1] (600 x 450).jpg
    IMG_20140503_174455[1] (600 x 450).jpg
    42.9 KB · Views: 8,901
  • IMG_20140503_174130[1] (600 x 450).jpg
    IMG_20140503_174130[1] (600 x 450).jpg
    43.4 KB · Views: 8,901
  • IMG_20140503_174001[1] (450 x 600).jpg
    IMG_20140503_174001[1] (450 x 600).jpg
    30.8 KB · Views: 8,901
  • IMG_20140430_215027[1] (450 x 600).jpg
    IMG_20140430_215027[1] (450 x 600).jpg
    38.2 KB · Views: 8,901
You are very talented. It took me countless hours to build my frame. You seem to be pretty fast! It is not your first project, right?
 
To me that cleaned up the lines nicely. If that short shock doesn't control the weight of a hubmotor very well, you can get rid of the extra tubing and fit the longer shock. I think that will improve the line even more, and cut out some unnecessary weight. It will also make it easier to sell when you are ready to do your next one, because the longer shock not only provides more travel, but it gives you more ability to tune the overall frame geometry. Being able to easily change the head tube angle and trail are important with ebikes, because it makes big differences in handling and high speed stability. It opens up the choices for fork selection too, because you can compensate for the effects of differences in travel and fork length.
 
hi,
acualy it is my first frame build.
the last bike was made of normal steet bicycle but is was burned.
becouse i was working on the balance leads and the whole pack burned down... only had +-1 month of fun out of it.
it was made from 18650 it was 15 ah 48v charged.

i started last week with the build on a wensday.
but it is going pretty fast.
the only time i can work on it is on monday,wensday,friday at night. or saturday if i dont work.

but i will thing about the rear suspention.
also it think the headtube from the cannondale is pretty thin. lik 1.5mm :?
i will give you a picture from that. so i am thinking to make a new head tube with a turning machine.

photo's later on today.
 
here some fhotos of my old bike
 

Attachments

  • fiets oud.jpg
    fiets oud.jpg
    47.3 KB · Views: 8,839
  • oud fiets 2.jpg
    oud fiets 2.jpg
    42.2 KB · Views: 8,839
hi
here are the pics please tell me if it is thick enough?
and also so welding picture's
 

Attachments

  • buisstuur.jpg
    buisstuur.jpg
    33.3 KB · Views: 8,808
  • buisstuur2.jpg
    buisstuur2.jpg
    33.1 KB · Views: 8,808
  • IMG_20140423_201959[1] (450 x 600).jpg
    IMG_20140423_201959[1] (450 x 600).jpg
    32.2 KB · Views: 8,808
Welding looks good. What thickness and dimensions have these tubes that you use?
A head tube made of CrMo steel is often 1.5mm thick. My head tube has the same thickness.
 
Back