drill bit had allot of drift and was blunt so i tried my 4.5mm new bit and munched through the side plate still some drift but i straightened up the edges with a file.
really didnt go acording to plan but its not too bad. as long as the side cover is balanced at the end its all good, just might look a bit shit if my vents arnt too straight.
really didnt go acording to plan but its not too bad. as long as the side cover is balanced at the end its all good, just might look a bit shit if my vents arnt too straight.