  1. Mogal

    Storage voltage for LiFePo4 cell?

    Sorry for bumping an old thread, but does this info still apply today? I have a 48V10AH LiFePO4 Aluminum Cased Battery (a little over a year old) and will be deploying for 6 months. What I pulled out of the thread is: My only means of measurement is my usage to work (or using a voltmeter) My...
  2. Mogal

    My build and experiences

    Got my first flat... kind of... Today was a weird day, I walked out from work at the end of the day to see a co-worker walking his electric bike home with a rear flat tire... I said "that sucks" he had a ride lined up to get home. I didn't notice anything with my bike until I got about 10 feet...
  3. Mogal

    My build and experiences

    Hi Beast, LOL Welcome home?! Thanks for the offer. Ever since I made the little brackets, I haven't had an issue and everything is staying nice and tight. The charger just shut off about 1/2 hour ago. I took the voltage reading. I got 54.4v straight off the battery. A little high for a 48 volt...
  4. Mogal

    My build and experiences

    I only have the stock charger that came with the kit. there is no way to monitor the actual activity of the battery. Is there a (Cheap) alternative to monitor the battery? The very first charge was about 48 hours. Since then, I've been leaving it plugged in after work, and unplug it in the...
  5. Mogal

    My build and experiences

    Thanks, I understand its not optimum, but it wouldn't fit the other way. With the home made brackets, its been 100%
  6. Mogal

    My build and experiences

    Hello, A small a-b-a-b speed test averages to 46km/h (28.5mph) on a small flat stretch (No peddling) The bike weighs 74 lbs (33.5kg) and I'm 195 lbs (88kg) Oh, and it is DEAD silent! I really can not hear it running! Amazing! I know the battery pack is good for 30amps, but would that get any...
  7. Mogal

    My build and experiences

    Al-right! so here is the (almost) complete bike. I've been riding it with the battery on the back end, and the stability is horrible! The battery does fit inside the frame but I can not plug in the charger when in the frame. So I need a means of quick removal. So I built a small rack that the...
  8. Mogal

    My build and experiences

    Here is my price list: If I had to do it again, I would not get the torque arm, as it doesn't seem to work well. The battery rack I would not get, as it won't span over the 700c tire/fender properly. Should have bought the freewheel with the kit, but not knowing any better LOL - couldn't find an...
  9. Mogal

    My build and experiences

    Sorry, longer post then I expected! Okay, I have the bike together! I've been learning LOTS about bikes!! I've been out on a ride, and have already had a couple of hang-ups... As you can see from the pictures, this frame wasn't designed for any power attachments! The MP4 axis kinda sits OUT...
  10. Mogal

    My build and experiences

    Alright! I got the kit! :lol:
  11. Mogal

    My build and experiences

    Hello all! I thought I would start this post for a little fun and to get some input as I proceed to build the bike (and for a question bank too!) This is my first ebike, and a little nervous about the build but excited about the ride and money savings (In the long run!) I'm building this for a...
  12. Mogal

    Your Creation's Before & After Pics

    Here is the before pic. I don't have an after pic, as I don't have the items yet. Specialized Crosstrail Disc (2015) Magic Pie 4 (VECTOR) 700c Rear Conversion Kit 48V10AH LiFePO4 Aluminum Cased Battery CatEye Velo Cycling Cumputer VELO-9 SolarStorm 5000lm 2x CREE XML U2 LED