I have a pack of 36 cells CALB 130AH , which I BB at 2.70v and after about 300 cycles /12000+ miles the cells are behaving exactly the same. When I am charging, I have cut off charge 124.2v (3.45/cell ) and when stop driving when the voltage is below 105v ( which usually never let it go that...