Looks like the new auction is open. The list of items is different this time.
https://svdisposition.hibid.com/catalog/530127/surplur-assets-to-the-ongoing-operations-of-coaster-cycles-2
My crank broke when I was pushing hard going up a hill. ruined my day. Lucky I can still walk. Don't remember the brand but it probably doesn't matter.