Hi, I bought a QS 138 90H 4kW motor kit with em150sp controller. The seller says that to get the required maximum speed (100kmh with 10 "wheels) the engine absorbs 86A continuous.
I currently have a 6S40P 22.2V 100Ah battery with bms 120A continuous/250A peak (INR18650 25E C cells) that I have been using for two months with the original 18V 1.5kW nominal, 3kW (peak) motor. Original motor absorbs around 130A at top speed and 210A during the hard acceleration (peak istantaneous over 300A). All tested with an amperometer DC.
I opened the battery because I want to rebuild it at 20S12P 72V30Ah and was wondering if I can get the required current from the motor and controller.
Searching for the code of my lithium cell on google, I obtained the manufacturer's data ( https://it.aliexpress.com/item/4001...82902508321701702241d25081956170131d-160d1605 ):
How many amps can I get from these cells in 20S12P configuration? How many amps can the bms votol em150sp withstand? I think it's 150A, right? Do I need a "common port" bms to use the regen function in braking? how many continuous and peak amps must the bms be in order not to break the controller in my setup?
Thanks everyone for the help, I can't do it alone.
I currently have a 6S40P 22.2V 100Ah battery with bms 120A continuous/250A peak (INR18650 25E C cells) that I have been using for two months with the original 18V 1.5kW nominal, 3kW (peak) motor. Original motor absorbs around 130A at top speed and 210A during the hard acceleration (peak istantaneous over 300A). All tested with an amperometer DC.
I opened the battery because I want to rebuild it at 20S12P 72V30Ah and was wondering if I can get the required current from the motor and controller.
Searching for the code of my lithium cell on google, I obtained the manufacturer's data ( https://it.aliexpress.com/item/4001...82902508321701702241d25081956170131d-160d1605 ):
How many amps can I get from these cells in 20S12P configuration? How many amps can the bms votol em150sp withstand? I think it's 150A, right? Do I need a "common port" bms to use the regen function in braking? how many continuous and peak amps must the bms be in order not to break the controller in my setup?
Thanks everyone for the help, I can't do it alone.