So I just bought 224 Samsung inr 25 r cells.

And I'm planning to build 3 battery packs 2 packs with 13 s5p for my friend and his wife and one 13s7p for my cargo/kid bike.
But I need a little advice concerning BMS and charger.

I am considering this one:
http://www.ebay.com/itm/48V-54-6V-13S-45A-Lithium-ion-Li-ion-Li-Po-LiPo-Polymer-Battery-BMS-PCB-System-/221740200277?pt=LH_DefaultDomain_0&hash=item33a0bef155

From Su power.

What I'm looking for is something both cheap, but also of good tested quality.

Any ideas ore suggestions?

I looking at 25A draw in current but will probably prefere to go with at least 40A BMS.

Any ideas for at power supply. Live in Norway and need 220 volt compatibility.

What size on Nikkelstrip do you suggest for welding. 10 mm*0.15mm ?

Best regards
Johannes :idea:
 
For welding and nickel size: -for parallel connections as this as possible, and for series connections I don't recommend nickel, solder copper wire on the nickel between the cells or weld copper sheet.

I had good experience with this BMS:

http://www.ebay.com/itm/Battery-Protection-BMS-PCB-Board-w-Balance-for-13-Packs-48V-Li-ion-Cell-max-25A-/251497839451?pt=LH_DefaultDomain_0&hash=item3a8e707b5b
 
That BMS is perhaps a litle bit ont the small size i current carrying capasity.
I have written to Bestech for a quote.
 