My new design of electric Longboard EF X2
The concept applies mainly motorholder to be compatible with the Truck Caliber II.

Material - powder coated steel and stainless steel (cheap and durable).
MotorHolder in the form of a rigid closed frame.

Version 1:
Inside is housed one engine and the electronics, ie. The ESC, switch, battery charge indicator.
Version 2:
Inside the 2 engines 6354 or shorter.
Zrzut%20ekranu%202016-06-17%2018.40.40_crs_zpst7it4doc.png

Zrzut%20ekranu%202016-06-17%2018.38.50_crs_zpscf0gfshw.png


The second element of the design is the battery box. The box is to enable the rapid exchange of packets (still in development).
 
Hi,
that looks really amazing. I really like the design. May i ask where you got this display from?
 
Looks like the same meter but is rated up to 80V and is $19.
http://www.ebay.com/itm/131630345531?_trksid=p2055119.m1438.l2649&ssPageName=STRK%3AMEBIDX%3AIT
 
Cheap option is the use of LiPo batteries.
Below is shown on the pictures koncepcja4 housings for 8 packages 5Ah Turnigy 3S, for a total of 20Ah / 6S
And so it established economic version of the long spacer :D
A range of about 40km (~ 25 miles)

Zrzut%20ekranu%202016-06-27%2023.32.09_cr_zpsorhedcl9.png

Zrzut%20ekranu%202016-06-27%2023.33.26_cr_zps4zefhzv5.png

Zrzut%20ekranu%202016-06-27%2023.32.49_cr_zps1ylhq9qh.png
 
I present the last version Lingboard with electric drive, a simple construction without a BMS, using conventional LiPo batteries.

087be2cedb22ae1e9ef8846b893de5f585aa8dd4.jpg

My English is poor, so I'll write a little, but instead will be a lot of pictures.

Components:
- DECK Globe - The Maiden
- Turnigy G160 245kV
- ESC FVT 120A 6S
- ZIPPY Flightmax 8Ah 6S (2x8Ah 3S)
- TRUCK - Caliber 2 44
- ABEC 11 Flywheels 83mm
- Remote Controller 2.4 Ghz nano

Technical parameters:
The maximum speed of 36km/h
Range up to 22km

MotorHolder made of stainless steel and PETG
Enclosure Lipo is printed with the PLA
Pulleys made from ABS+ on a 3D printer

20161014_172914_HDR_cr_zpspmk2ywm6.jpg

x2-4_zpsvftjcohe.jpg

755cc5fce27fc7da0625a4c9cab73d4c3ed45d57.jpg


MotorHolder apart from the motor also includes ESC, the receiver RC and switch
bc4ebaa6a0ddd32385bb57eff91a5bd4bca999ed.jpg

27733f5641d5ac881f2ec5a80ee3e288041f72a0.jpg

However, you can mount a large motor such as SK3 6374
5b4102d94919b7273bc50077da674496116a5f01.jpg

Or two smaller ones such as SK3 6354
5057b0cbb54a8f45c8fc38c14f9aee2b83afc226.jpg


I did also versions of the motor holder for Paris180
28b6759a41608c35ac40dacf8458f79f32da188d.jpg

5719d763314a53163b94dc75ccb2a11300c3ded5.jpg


Transmission belt HTD5M has a ratio of 15/36

Pulleys printed on a 3D printer with ABS
I produce pulleys for ABEC 11 Flywheels and Kegel Orangatang
5d4d75a45c142ba17c23821342642595f784f65e.jpg

d6b9ae2be7876dd4cb822b3c6a7e61e09bf24a06.jpg

c33ee8c194a72eef69336566b4eb28840e1fa0ab.jpg

bb2d68450b92bb4ba7be0a0a775e42a9840b31ad.jpg


Enclosure Lipo is printed with the PLA it contains LiPo ZIPPY Flightmax 2x8Ah 3S and capacity indicator
b69bc89732f856ef63acdbfe5b506ebe767559d7.jpg

12_zpsnqugvia5.jpg


Sorry for my english if something is not understandable :?
 
Nice design idea, however I would not recommend putting the esc close to your bldc motor unless you shield the circuitry very well.
The electromagnetic field around your motor can easily disrupt your esc causing weak or unstable signal if you have the receiver nearby as well. It can also cause random logic problems on the cpu as well as on the memory. You can fix this if you properly shield it though.
 
WTech said:
Nice design idea, however I would not recommend putting the esc close to your bldc motor unless you shield the circuitry very well.
The electromagnetic field around your motor can easily disrupt your esc causing weak or unstable signal if you have the receiver nearby as well. It can also cause random logic problems on the cpu as well as on the memory. You can fix this if you properly shield it though.

It's logical what you write, but I have not noticed problems with the receiver and the ESC, and not only for himself made this motor holder.
 