Hi I have a Performer sports recumbent trike . I took it out for a spin tonight and it felt a bit loose in the arse end. I had a bit of a look and couldnt see anything. When I got home I had a good look and found that my frame has cracked on what would be the equivalent of the seat stay on a normal bike. Does anyone know where to get it strengthend and repaired in Melb cheers Alan.
 
http://www.gripsport.com.au/

They repaired a cracked aluminium MTB for me in the past, welding the crack at the headtube, adding gusseting and powdercoating the whole frame after. I also had them add a rear disk mount to a cromo hardtail and then powdercoat. Both were nice jobs, neither super cheap though.
 
Thanks very much for that. I dropped off my frame today I thought the price was pretty good $140 to repair and add some strengthenig tubes thanks Alan :D
 