Awsome sunny 18 celcius out there today, amazing weather, i decide to top off the chopper for a ride...... get the lightbulb rack to drain a bit and then re-fill them, put the CA on the 24 cell PSI pack and no life to the CA.....
'
Get my volt meter, check voltage, 0.150 mv
Somehow, the Soneil chargers, being connected to the pack for 3 weeks, have managed to drain it completely.
There goes 1000$ :|
![Shock :shock: :shock:](/sphere/data/assets/smilies/icon_eek.gif)
'
Get my volt meter, check voltage, 0.150 mv
![Shock :shock: :shock:](/sphere/data/assets/smilies/icon_eek.gif)
![Shock :shock: :shock:](/sphere/data/assets/smilies/icon_eek.gif)
![Shock :shock: :shock:](/sphere/data/assets/smilies/icon_eek.gif)
Somehow, the Soneil chargers, being connected to the pack for 3 weeks, have managed to drain it completely.
![Evil :evil: :evil:](/sphere/data/assets/smilies/icon_evil.gif)
There goes 1000$ :|