Hi. I built a triangle-shaped glue-pack 18650 battery pack, but I'm having trouble finding a supplier of the size of PVC heat shrink wrap I need. Considering the dimensions of my pack I need PVC heat shrink wrap that is 370-400 mm wide laying flat. The desired thickness could be anywhere from 10-30 mils (.25 to .8 mm).

Again, I am having trouble finding a supplier. Can anyone provide any suggestions for one?

Thanks in advance.
 
mistercrash said:

Thanks for the info. Yesterday, someone pointed me to some similar heat shrink tubing available on AliExpress, which I purchased. Unfortunately, the wrap I found, as well as that posted for sale on your Ebay links are very thin-walled, and probably will require at least three layers to provide a decent level of protection.

Thanks again.
 