Nissan Leaf Cells Test Data

.??..you do know the leaf uses "pouch" cells , not 18650 cells ??
Why wouldnt they be rated for 1200 cycles ? They are purpose developed and made specifically for the Leaf and presumeably tested to enable that claim to be made.
....And there are several 18650s with similar and higher cycle life figures.
 
Offroader said:
Just wanted to ask you guys does anyone know why these cells are rated at 1200 cycles to 80% capacity?

Why so high when most 18650 cells only have about 500 cycles to 80% capacity?

I can give you one answer based on my measurement and observation. There are two general categories of Li-Ion cell.
1) Best available energy density cells
2) "Robust or durable" cells

The first category is characterized by maximum achievable energy density at a given time. However, at a cost of lower cycle and lifetime, lower power density and intrinsic safety. We are talking about 700Wh/l for modern cells in 18650 size. It should be also noted, that there were made no significant progress in increasing energy density here from 2012.

The second category is logically an opposite to the first. So those cells are very good in every aspect exept the energy density. But in this category was made a huge progress. From 2012 it starts at 314Wh/l (Leaf 24kWh cells) for best pouch cells and now in 2016 we have about 550Wh/l (new LG cells).

So you can not compare Leaf cell and a modern high density 18650 cell. But I an quite sure that you can find a 1500mAh (320Wh/l) 18650 cell (e.g. for power tools) which will have the same or even beter cycle life and other parameters than Leaf cell.
 
Sorry to hijack the thread but I have a potentially serious concern.

I have 12 modules / 24s of 2012 AESC modules from a Leaf in my motorbike. Today just before making the last connection from positive to the contactor I accidentally touched the lead to the chassis, had a spark and some copper welded. The chassis is obviously not supposed to carry HV-, not even 12V-, typical on a motorbike.
At first I suspected the negative lead around the fuse and the Kelly controller, but they have no continuity to ground. A full short at 92V would have been much more disastrous and should have blown the fuse. With a multimeter I measured voltages of up to 1.6V to ground from various points of the pack. The voltage only registers briefly.
I disconnected all the leads and even the interconnect to isolate - no luck.
I removes the lower 4 modules and took the whole harness off.
Now I can measure from various points and have the same thing all over the place, nearly every 2nd connector register 0.1-0.3V briefly, even on the 4 modules that are now completely removed from the bike. Double-checked with a 2nd multimeter as I thought I'm going crazy.

I am suspecting that the exposure to the elements has breached some kind of seal and I have a "bit of a short" to the cans. The obvious questions:
- Can anyone else confirm this?
- Is this a big issue? HV leads anywhere have to be handled carefully anyway. Kelly & contactor will be driven by dedicated LV pack, but should I isolate the controller from ground? They are known to have some ground issues. I could isolate the individual modules on the lower pack, but the upper one is a bespoke, tight fit...
- Anything else i should test?

A picture:
 
marcexec said:
Now I can measure from various points and have the same thing all over the place, nearly every 2nd connector register 0.1-0.3V briefly, even on the 4 modules that are now completely removed from the bike. Double-checked with a 2nd multimeter as I thought I'm going crazy.

I am suspecting that the exposure to the elements has breached some kind of seal and I have a "bit of a short" to the cans. The obvious questions:
- Can anyone else confirm this?

Hi!
I just now tested my Leaf 2012 modules and there is a consistent reading of 20mV between any battery lead and the aluminum can... :idea:
Didn't check the current involved, but it is real, since contacting 2 different parts of the module can gives exactly 0mV.
In my case I suppose it is nothing to worry about. I bought them in 2013. It is just a few days that I put them in operation in my e-bike.
They sitted untouched for 5 years and they lost a fairly small amount of charge, very evenly accross all cells.

Have fun!
 
1jw3o0.jpg


This is a picture of one of the 2 battery packs created filling Decathlon side bike packs with Nissan 2012 modules.
For an e-bike that is having a range of 200km at 35kmh speed.

Have fun!
 
Is it just one can out of several that's showing leakage between can and terminal?

Unrelated, but I'd put some insulation around the barrels of those crimp terminals to stop them touching the casing if bent!
 
Punx0r said:
Is it just one can out of several that's showing leakage between can and terminal?

Unrelated, but I'd put some insulation around the barrels of those crimp terminals to stop them touching the casing if bent!

I was answering to marcexec... He has some leakage, mine seems ok...

I didn't put insulation around the barrels of those crimp terminals, since there is no chance they can be bent enough to contact the can...
It seems close in the picture, but really the clearance is huge... And I use the barrel of the terminals to probe and balance the single cells...
It is very convenient...

Have fun!
 
The new 62 kWh Leaf is coming out soon. The cells are still made by AESC, not LG. I have not heard what the chemistry is, but I have to guess it is now NMC.

The pack is 288 cells, 96s3p. The sardine cans are gone. The plastic framed cells are presumably welded together in threes, and are stacked in frames holding 27, 12, or 21 cells each.

https://d2t6ms4cjod3h9.cloudfront.net/wp-content/uploads/2019/01/LEAF_e_Battery_9-source-898x599.jpg

https://d2t6ms4cjod3h9.cloudfront.net/wp-content/uploads/2019/01/LEAF_e_Battery_1-source-898x599.jpg
 
Suprise lets revive:
I have 5 Nissan 2018 cells in 4s 2p configuration per pack.
Does anyone know how much amps I can draw from it in this 2018 version?
All information I found was on this website, but no info about max. Amps per module.

https://pushevs.com/2018/01/29/2018-nissan-leaf-battery-real-specs/

Cheers, Elias
 
Warren said:
The new 62 kWh Leaf is coming out soon. The cells are still made by AESC, not LG. I have not heard what the chemistry is, but I have to guess it is now NMC.

The pack is 288 cells, 96s3p. The sardine cans are gone. The plastic framed cells are presumably welded together in threes, and are stacked in frames holding 27, 12, or 21 cells each.

https://d2t6ms4cjod3h9.cloudfront.net/wp-content/uploads/2019/01/LEAF_e_Battery_9-source-898x599.jpg

https://d2t6ms4cjod3h9.cloudfront.net/wp-content/uploads/2019/01/LEAF_e_Battery_1-source-898x599.jpg
Your photo links are broken Warren. But there is a detailed review here...
https://insideevs.com/news/342009/here-is-the-nissan-leaf-e-62-kwh-battery-video/
 
DasDouble said:
Suprise lets revive:
I have 5 Nissan 2018 cells in 4s 2p configuration per pack.
Does anyone know how much amps I can draw from it in this 2018 version?
All information I found was on this website, but no info about max. Amps per module.

https://pushevs.com/2018/01/29/2018-nissan-leaf-battery-real-specs/

Cheers, Elias
If you flick back a page or so on this thread to posts starting in Jan 2016,..you will find reports of these cells being tested at 10 = 11C .
But that will depend on your individual situation, enclosure, burst or continuous load, how much voltage sag you can tolerate, etc
Read,.. and make your own conclusions.
 
Hi, guys. Awesome to see many battery experts in this group.

I was wondering to use Nissan Leaf battery capacity to supply energy to home appliances. However, I don't find battery specs with a graph or table showing the reduction of capacity (kWh) x power or current consumption as a function of time duration or a simple current x time duration. I am not an expert in batteries, but I believe that even modern batteries as the ones used in Nissan leaf lose capacity in the discharging rate increase due to the internal resistance, isn't it? I really appreciate any help and some good references about the use of EV for home applications, specially about Nissan leaf, that I am interested in. Regards!
 
Hi everyone, I have an EV conversion I've done with a 62kwh leaf pack. I was wondering if anyone had any information on the maximum discharge current from this pack so I can implement safety measures, making sure I don't damage it. I've already pulled up to 400amps for a short time, which I know is the most the leaf inverter would have pulled. How far above that number is safe?
 
I have an EV conversion I've done with a 62kwh leaf pack.
Are you using it in the original configuration ,..355v, 168 ah ?
If so, your 400 a draw ,( < 2.5 C ) , is well within its designed performance.
Those cells are claimed to be an “improved” version of the original Leaf cells, which, according US Department of ENERGY study, those original 54Ah packs could provide up to 240A continuous or over 540A short time on pulse, (10+C discharge),..so it should be reasonable to expect similar or better capability from the cells in your pack.
HOWEVER,..im sure you are aware that test results , and daily use are very different situations, and that one of the issues with Leaf packs is lack of active cooling which would be desirable in high discharge situations, so some caution is advised !
But, drawing 3-4C, ( 650a) should be feasible, at least for short periods.
Unless you can find some reliable data from other users who have tested the pack at higher discharges, (400+a), you might want to monitor internal pack temperatures , voltage sag, etc etc to be sure nothing nasty is happening.
How far above that number is safe?
..? ..that depends on your definition of safe, and what your risk threshold is !
Some people do not think any Lithium pack is “safe” , even when just sitting unused !🙄
 
Yes, using it in the original configuration. It's great news that I should be able to draw even close to 650A. I'm working on installing temperature sensors right now but the batteries are not getting anywhere close to warm to the touch at the moment. I'm only driving for short bursts though, I'm not able to drive the car on public roads yet. I did some data logging with my BMS of cell resistance and voltages if you're interested in taking a look. After I get temperature sensors installed I will do some more extensive data collection. Thank you for your response!!

 