http://www.eurekalert.org/pub_releases/2011-06/uotf-uot062411.php
Nature Photonics looks like a pretty cool publication. They have made this months Technology Focus section available as a pdf:
http://www.nature.com/nphoton/journal/v5/n5/pdf/techfocus.pdf
Amazing work going on w/solar panels etc!
1OCk
Public release date: 26-Jun-2011
Contact: Takara Small
takara@ecf.utoronto.ca
416-946-7257
University of Toronto Faculty of Applied Science & Engineering
http://www.engineering.utoronto.ca/home.htm
U of T researchers crack full-spectrum solar challenge
In a paper published in Nature Photonics, U of T Engineering researchers report a new solar cell that may pave the way to inexpensive coatings that efficiently convert the sun's rays to electricity.
The U of T researchers, led by Professor Ted Sargent, report the first efficient tandem solar cell based on colloidal quantum dots (CQD). "The U of T device is a stack of two light-absorbing layers – one tuned to capture the sun's visible rays, the other engineered to harvest the half of the sun's power that lies in the infrared," said lead author Dr. Xihua Wang.
"We needed a breakthrough in architecting the interface between the visible and infrared junction," said Sargent, a Professor of Electrical and Computer Engineering at the University of Toronto, who is also the Canada Research Chair in Nanotechnology. "The team engineered a cascade – really a waterfall – of nanometers-thick materials to shuttle electrons between the visible and infrared layers."
According to doctoral student Ghada Koleilat, "We needed a new strategy – which we call the Graded Recombination Layer – so that our visible and infrared light-harvesters could be linked together efficiently, without any compromise to either layer."
The team pioneered solar cells made using CQD, nanoscale materials that can readily be tuned to respond to specific wavelengths of the visible and invisible spectrum. By capturing such a broad range of light waves – wider than normal solar cells – tandem CQD solar cells can in principle reach up to 42 per cent efficiencies. The best single-junction solar cells are constrained to a maximum of 31 per cent efficiency. In reality, solar cells that are on the roofs of houses and in consumer products have 14 to 18 per cent efficiency. The work expands the Toronto team's world-leading 5.6 per cent efficient colloidal quantum dot solar cells.
"Building efficient, cost-effective solar cells is a grand global challenge. The University of Toronto is extremely proud of its world-class leadership in the field," said Professor Farid Najm, Chair of The Edward S. Rogers Sr. Department of Electrical & Computer Engineering.
Sargent is hopeful that in five years solar cells using the graded recombination layer published in today's Nature Photonics paper will be integrated into building materials, mobile devices, and automobile parts.
"The solar community – and the world – needs a solar cell that is over 10% efficient, and that dramatically improves on today's photovoltaic module price points," said Sargent. "This advance lights up a practical path to engineering high-efficiency solar cells that make the best use of the diverse photons making up the sun's broad palette."
The publication was based in part on work supported by an award made by the King Abdullah University of Science and Technology (KAUST), by the Ontario Research Fund Research Excellence Program, and by the Natural Sciences and Engineering Research Council (NSERC) of Canada. Equipment from Angstrom Engineering and Innovative Technology enabled the research.
To read the published paper in its entirety, please contact Takara Small, Communications & Media Relations Coordinator for the Faculty of Applied Science & Engineering, University of Toronto.
For more information, please contact:
Takara Small
Communications & Media Relations Coordinator
Faculty of Applied Science & Engineering, University of Toronto
416-946-7257 or cell 416-985-6839 | takara@ecf.utoronto.ca
Nature Photonics looks like a pretty cool publication. They have made this months Technology Focus section available as a pdf:
http://www.nature.com/nphoton/journal/v5/n5/pdf/techfocus.pdf
Amazing work going on w/solar panels etc!
1OCk