Sorry, no ebikes to see here, just a few pics from around my shop. While I always encourage DIY, sometimes it's worth paying a few bucks for professional results. I have personally witnessed a racecar go into a wall due to a failed weld, and the results weren't pretty. Upon inspection, the...