Yeah I got the 18650 nese kit from that mad scientist Now what cell it needs a flat top my controller does 80amps and I like headroom ?
I wanted Samsung 30q but some leak so now what ?
I would like to buy from IMR Texas us of a. But don't care I just don't want to buy sells they're ripped out of an almost new pack. I want new cells.
 
999zip999 said:
Can't anyone help me with a suggestion for a 18650 cell as 8p for 80amp controller ?

25R's are a great cell.
Samsung INR18650-25R which are 2500mAh and max cont 20A discharge

https://lygte-info.dk/review/batteries2012/Samsung%20INR18650-25R%202500mAh%20%28Green%29%20UK.html
 
Yes as price is right 3.75 over one hundred. plus they've been around for a while and I would have heard about the complaints if there was some. But I just got a pack of 20s 6p Samsung 40 t and not sure if they're all they're cut out to be. Melted a edge 1500 dd motor so have to re-lace a muxus 3000 for further testing.
Thanks Mark z

,
 
25R are darn good but I can find them for 3.15 euro for 100, save 0.10E for 200
20R is 1.19 euro
Maybe look into PF or 35E, 29E, MJ1, VTC and see what prices you get and compare for your needs. VTC is a good price, or was I havent been paying attention for the last year.
 
Markz the first three cells you mentioned are 10a cells I need 15a or better . The Sony cells are good but 6 USD. And 3.15 euro is 3.80 usd or about the same price.
 
999zip999 said:
Markz the first three cells you mentioned are 10a cells I need 15a or better . The Sony cells are good but 6 USD. And 3.15 euro is 3.80 usd or about the same price.

Check out sanyo:
https://www.candlepowerforums.com/vb/showthread.php?421805-Test-Review-of-Sanyo-Panasonic-UR18650NSX-2600mAh-(Red)

https://www.imrbatteries.com/sanyo-ur18650nsx-2600mah-20a-flat-top-battery/
Capacity is not the best but its high power and since you want it cheaper, might be a good option.
3.35$
 