2 to 3 times the weight; 2 1/2 times the distance; greater maximum discharge capacity, depending on the cells used.So what's the advantage of 63ah over 24ah? Capacity (distance)?
Possibly. It depends on the cell type being used, assuming you need 150A. The 24Ah pack would need to be comprised of high output cells, like a Samsung 25R (if the pack is going to be made of 18650 cells). That would be 10P, and the cell has a rated output 20A. That would support 200A continuous. 200 cells is a big pack. You can use a lower discharge, higher capacity cell for the 63Ah pack. If you used a 35E cell, you'd need 18P to meet energy requirement, but 19P to meet the 150A discharge; so 380 cells total. The trick is to choose the right cells, that when in parallel can provide the discharge amps that you need, but also store the amount of energy that you need, using the least number of cells. You also have choices between 18650 and 21700 cells, and it may make sense to go with the latter. Lastly, this assumes you are going with lithium ion batteries. If you are comfortable with using Lipo batteries and the higher risk associated with them, then you could put together a configuration that meets the requirements, but with a lot less weight than a 200 cell 18650 pack.Will 63ah work with below configuration?
2 to 3 times the weight; 2 1/2 times the distance; greater maximum discharge capacity, depending on the cells used.
Possibly. It depends on the cell type being used, assuming you need 150A. The 24Ah pack would need to be comprised of high output cells, like a Samsung 25R (if the pack is going to be made of 18650 cells). That would be 10P, and the cell has a rated output 20A. That would support 200A continuous. 200 cells is a big pack. You can use a lower discharge, higher capacity cell for the 63Ah pack. If you used a 35E cell, you'd need 18P to meet energy requirement, but 19P to meet the 150A discharge; so 380 cells total. The trick is to choose the right cells, that when in parallel can provide the discharge amps that you need, but also store the amount of energy that you need, using the least number of cells. You also have choices between 18650 and 21700 cells, and it may make sense to go with the latter. Lastly, this assumes you are going with lithium ion batteries. If you are comfortable with using Lipo batteries and the higher risk associated with them, then you could put together a configuration that meets the requirements, but with a lot less weight than a 200 cell 18650 pack.
Research the cells since the ratings don't tell the whole story. For instance, I wouldn't build a high discharge pack with 35E cells. Although they can output 8A, per the spec sheet, voltage sags a lot at that level. The 25R would sag a lot less, and the lipos have almost no sag when they are greater than half charged.
Unknown at the moment. Everywhere I see they just have it listed as 72v 63Ah battery. If I get that info I will post. ThanksMost important what model number and name of cell going into the pack ?
This is the most important part. !
If the cells are brand name, they would describe them prominently in their listing. Otherwise you can virtually guaranty that they are generic Chinese cells.Unknown at the moment. Everywhere I see they just have it listed as 72v 63Ah battery. If I get that info I will post. Thanks
The math doesn't work. Those dimensions seem to be too small for a 72V 63Ah battery. Assuming high energy 18650 cells (~360), the volume would be significantly larger.Are there any good web sites where they can build custom battery?
My battery is 13" Length (330mm) x 6" Height (152mm) x 5" Width (127mm)
ok, Thanks. So it wouldn't work unless there's high energy cells. I currently have 72v 24Ah battery and that's what those dimensions are.The math doesn't work. Those dimensions seem to be too small for a 72V 63Ah battery. Assuming high energy 18650 cells (~360), the volume would be significantly larger.
Not necessarily. They don't state the dimensions of the 63Ah pack, but it looks like the frame can support quite a few cells. Looking at the specs page, it looks like you need the big battery to have fun on that bike and I'd probably still have range anxiety.ok, Thanks. So it wouldn't work unless there's high energy cells. I currently have 72v 24Ah battery and that's what those dimensions are.
So if you look at this website, they have option for 72V 63Ah battery and I do have Eagle. So they must be using high energy cells than.
Cab Eagle, Eagle Electric bike - Cab Motorworks
The 2023 CAB Eagle has unbeatable torque, nimbleness, and resilience. Shop today at cabmotorworks.com or call us at 714-594-9885.www.cabmotorworks.com
On my first ride I didn't know what the range was, but after that on 72 24Ah battery I can do 45 miles (full acceleration occasionally) . If I go easy, I can do 55 miles of range on it. So thats why I'm looking in to 72v 63Ah battery to see if I can get more range out of it. I'm trying to see if I can get it somewhere else, because $2500 that they have it listed is a bit too much for me.Not necessarily. They don't state the dimensions of the 63Ah pack, but it looks like the frame can support quite a few cells. Looking at the specs page, it looks like you need the big battery to have fun on that bike and I'd probably still have range anxiety.