Planet Indigo
100 mW
- Joined
- Sep 22, 2018
- Messages
- 40
This is my first ebike conversion and I'm very worried about my battery.
I received my battery/charger yesterday and before installing it on the bike, I wanted to make sure all fit and worked perfectly.
I inserted the charger connector inside the battery connector and big sparks started flying, I removed the connector immediately but the charger connector is singed and im not sure if the battery connector is supposed to look like this on the inside. For the record, the battery power switch was off (little circle O, not -) since I had heard that batteries should be charged while off.
I attached two pictures.
After googling some it appears that ebike batteries are a rare exception where it's better to plug the charger in the wall first before inserting the plug in the battery. I'm double surprised because it goes against my previous experience with batteries and my seller's instructions were to plug the charger and battery before wall socket...
The cells still seem to have voltage since the battery indicator still reports 1 green light (same as when I received it). My first priority at this point is to not damage the battery cells. I am very afraid of plugging them together now. The charger has a light indicator, and when I plug it alone in the wall socket, the light stays off, is the light supposed to be off when plugged in and only on when charging? Or on in both cases? Should I try to "clean up" the inside of my battery charging port? Is it supposed to look like this on the inside?
I would very much appreciate any advice on what is my safest next course of action given that my priority is not to damage the cells. Thanks.
I received my battery/charger yesterday and before installing it on the bike, I wanted to make sure all fit and worked perfectly.
I inserted the charger connector inside the battery connector and big sparks started flying, I removed the connector immediately but the charger connector is singed and im not sure if the battery connector is supposed to look like this on the inside. For the record, the battery power switch was off (little circle O, not -) since I had heard that batteries should be charged while off.
I attached two pictures.
After googling some it appears that ebike batteries are a rare exception where it's better to plug the charger in the wall first before inserting the plug in the battery. I'm double surprised because it goes against my previous experience with batteries and my seller's instructions were to plug the charger and battery before wall socket...
The cells still seem to have voltage since the battery indicator still reports 1 green light (same as when I received it). My first priority at this point is to not damage the battery cells. I am very afraid of plugging them together now. The charger has a light indicator, and when I plug it alone in the wall socket, the light stays off, is the light supposed to be off when plugged in and only on when charging? Or on in both cases? Should I try to "clean up" the inside of my battery charging port? Is it supposed to look like this on the inside?
I would very much appreciate any advice on what is my safest next course of action given that my priority is not to damage the cells. Thanks.