Apologies for the OT, but:
Hmmm....
http://www.endless-sphere.com/forums/viewtopic.php?f=30&t=32838
I haven't measured them, but they are about the width of my pointer-finger's length.
Now I wonder what kind of power I can get out of that thing.
EDIT: Added measurements:
Stator: 50mm width, 170mm diameter
Magnets: 53mm width, 171mm diameter (0.5mm airgap at most)
oatnet said:
Hmmm....
http://www.endless-sphere.com/forums/viewtopic.php?f=30&t=32838
I haven't measured them, but they are about the width of my pointer-finger's length.
Now I wonder what kind of power I can get out of that thing.
EDIT: Added measurements:
Stator: 50mm width, 170mm diameter
Magnets: 53mm width, 171mm diameter (0.5mm airgap at most)