Hello, I have a zero10x escooter equipped with a 23AH LG 14s7p 52v.
I have a problem since last year, the battery shuts off while I was driving (I didn’t have the acceleration even half way and the battery had 53v and it was not hot) and after a few minutes it shuts on and the voltage are comming back and all seems normal. I thought that the BMS would be damaged and I changed it with a completely different one (the original one had a 50Ah discharge and a separate discharge/charge port and the new one is a 60AH daly BMS with a common discharge and charge port) and the first trip with a fully charged battery I could drive about 10 km and the battery dies again. After a few days I drove it again and was able to drive 300m and died again, after few minutes all seems normal and just some meters away dies again.
First time I thought it was a bad BMS and the second option and the last is the battery cells, but how do I know which ones are bad? When I changed the BMS I measured all the battery series and nothing was wrong, no corroded or run down batteries. Cables look ok, the battery had 2 fuse for each xt60 connector and they are also ok.
I test it again yesterday with wheels in the air and all was normal, the problem appears only with my me on the escooter.
What should I do next?
I thought of opening the battery pack and taking each cell separately and then see if I have dead/bad cells, and give them a maximum charge and a discharge to see how many mAh they have. But this is a lot of work to take each one separately they are 98 cells , do you have another suggestion?
Can I test parallel cels separately? Or to one side I must to take off the nickerl strip?
I have a problem since last year, the battery shuts off while I was driving (I didn’t have the acceleration even half way and the battery had 53v and it was not hot) and after a few minutes it shuts on and the voltage are comming back and all seems normal. I thought that the BMS would be damaged and I changed it with a completely different one (the original one had a 50Ah discharge and a separate discharge/charge port and the new one is a 60AH daly BMS with a common discharge and charge port) and the first trip with a fully charged battery I could drive about 10 km and the battery dies again. After a few days I drove it again and was able to drive 300m and died again, after few minutes all seems normal and just some meters away dies again.
First time I thought it was a bad BMS and the second option and the last is the battery cells, but how do I know which ones are bad? When I changed the BMS I measured all the battery series and nothing was wrong, no corroded or run down batteries. Cables look ok, the battery had 2 fuse for each xt60 connector and they are also ok.
I test it again yesterday with wheels in the air and all was normal, the problem appears only with my me on the escooter.
What should I do next?
I thought of opening the battery pack and taking each cell separately and then see if I have dead/bad cells, and give them a maximum charge and a discharge to see how many mAh they have. But this is a lot of work to take each one separately they are 98 cells , do you have another suggestion?
Can I test parallel cels separately? Or to one side I must to take off the nickerl strip?