gopro drone battery 0v

goatman

10 MW
Joined
Jun 23, 2019
Messages
3,214
Location
Surrey, B.C.
sold the drone awhile ago but couldnt find the spare battery
i found it at 0v
couldnt find anything about opening them up so i just ripped into it
you only need to pop the top off

IMG_20210407_165529.jpg

IMG_20210407_165713.jpg

IMG_20210407_165838.jpg

IMG_20210407_165928.jpg

IMG_20210407_170004.jpg

cant see anything wrong

IMG_20210407_170222.jpg

IMG_20210407_170448.jpg

IMG_20210407_170454.jpg
 
the leds werent working before but now i have 3 out of 4 on the meter

IMG_20210407_183447.jpg

ive got power all the way upto these chips

IMG_20210407_170725.jpg

IMG_20210407_170454.jpg

i think all i need to figure out now is which of these wires turns on the board

IMG_20210407_183611.jpg

black purple and green are negative
blue is positive
black and purple to blue is 14.74v
green to blue is 15.35v