Spacey
100 kW
I've had suprisingly good results using chemical metal over a torque arm in the weird dip in my Cannondale Gemini swinging arm. The torque arm originally just sat in the middle of this big space so I put duct tape over the swinging arm and made a mold using the chemical metal with the torque arm in place on the axle.
Once it set is was very strong and comes away very easily due to the duct tape not sticking to the chemical metal. The fit is very tight althoug the actual torque arm whilst thick enough has a bit of play in the axle slot as it is a tiny bit too big, so I don't use regen at the moment.
I am dumping 40 amps 66v of hard acceleration using the new HS3540 motors that pull a lot harder than the 9C 2807 that was on there.
Once it set is was very strong and comes away very easily due to the duct tape not sticking to the chemical metal. The fit is very tight althoug the actual torque arm whilst thick enough has a bit of play in the axle slot as it is a tiny bit too big, so I don't use regen at the moment.
I am dumping 40 amps 66v of hard acceleration using the new HS3540 motors that pull a lot harder than the 9C 2807 that was on there.