hi
There seems to be a short cut to building a battery for those able to get a module like this one
they are already spot welded in place so i imagine that this is a short cut already done step. how easier does starting with a module like this is ? is it really faster or is there some cell dissasembling to do
1 apart from adding a bms what is there to add to add safety feature or usefull feature while being in there?
2 do each cell needs to be tested? how and what parameter to respect
3 is balancing steps required?
4 what should one be aware of before starting with such a module?
thanks
im a noobish but read alot
There seems to be a short cut to building a battery for those able to get a module like this one
48v 16s3p A123 26650 Lifepo4 Module 52.8v 7.5ah 396wh
It's very rare to find 16s Lifepo4 48v modules like this. They are very clean and made of A123 ANR26650M1B cells. There are a total of 48 cells in 16s3p configuration. All you need is a T-15 security bit that is at least 2" long to open the case. There are 14 screws. The case comes off easy, no...
batteryhookup.com
they are already spot welded in place so i imagine that this is a short cut already done step. how easier does starting with a module like this is ? is it really faster or is there some cell dissasembling to do
1 apart from adding a bms what is there to add to add safety feature or usefull feature while being in there?
2 do each cell needs to be tested? how and what parameter to respect
3 is balancing steps required?
4 what should one be aware of before starting with such a module?
thanks
im a noobish but read alot