I had same issue of lack voltage. Cycled in and out of app. Left bike on few minutes with app off went back in app, app now getting correct readings from controller.
Update. Controller has been turned up to 80 amps dc and running fine somewhat. Only problem is if I crank throttle from slow or stop controller cuts out but thats for another thread. Problem was hall wires. Reran hall test and kept failing. Tried 10 to 30 amps for the test. Finally...
I made 4 5s10p batteries as pictured below. Made 3 on the left and 1 on the right. I made them using the copper nickle method, using .15mm nickle and .1mm copper. They are made like this so I can use them on another bike as a 15s. The current bike I am using them for I run as a 20s, but I...
Update. I have changed some of my settings. Now bike tops out on the flat 40mph with no flux and doesn't cut out. I have posted screen shots of changed settings. I would think I could run it higher the amps and get a top speed of 45 to 50, but maybe I am wrong, not that I really would...
I forgot to add motor is qs205 4T v3. And I used SB50 connectors. I have some xt 150 connectors I can switch them out, but i believe the xt150 are made for 8awg. And I would have thought the SB50 connectors seem more beefy than a xt150.
When I take my bike up to 30 mph the controller cuts out. Not sure if its my settings or my battery. Battery is 20s10p lishen cells no BMS diy with copper nickle sandwich(.1mm copper plate across both series and parallel connections) and for cable connections i soldered 2 6awg wire to the .1mm...
Quick question for separate regen hook up. Is attaching a separate throttle and connecting the 5v ebrake wire(signal) and then +5 and ground all I need for the slide regen to work. Or do I have it wrong and slide regen works only when hooked up to your throttle and u stop acceleration then the...
Does it matter if I put the precharge resistor on the negative side? I was taught when connecting a battery positive then negative. And when removing a battery negative then postive.
Did u ever figure out the difference between hard start and boost. And what settings they affect. Been looking for what the difference is and I have not found much info on the topic.