Well, it seems they keep failing and coming my way.. izip .. schwinn.. Raleigh.. Giant.. now iGo's !
This poor iGo came to me a couple months ago with battery issues, moisture got in there and caused the BMS to shut down, after checking all cell voltages and sun drying for a while it came back...