Recently I've been working on various golf carts, converting to lithium, swapping motors and even full brushless conversion.

Saw this thing sitting at a workshop, tracked down the owner and bought it for a friend. The mechanic told me that the batteries were dead and that the brushes from the motor were probably gone as well. I had a new brush set so I thought this would be an easy job...

I opened it up today to find this :shock:



The controller is shorted internally as well :flame:




Guess it's time for a full lithium/brushless conversion 8)

Update: 26/08/
I've finally made some progress, mounted the motor and controller. More pictures to follow.
 

Attachments

  • IMG_20221229_121150.jpg
    IMG_20221229_121150.jpg
    4.9 MB · Views: 297
  • IMG_20221229_121147.jpg
    IMG_20221229_121147.jpg
    4.3 MB · Views: 296
  • IMG_20221229_121145.jpg
    IMG_20221229_121145.jpg
    4 MB · Views: 292
  • IMG_20221229_121142.jpg
    IMG_20221229_121142.jpg
    4 MB · Views: 292
  • IMG_20221229_121125.jpg
    IMG_20221229_121125.jpg
    4.4 MB · Views: 291
  • IMG_20221219_121610.jpg
    IMG_20221219_121610.jpg
    3.5 MB · Views: 290
  • IMG_20221219_121629.jpg
    IMG_20221219_121629.jpg
    3.9 MB · Views: 288
  • IMG_20230825_122853.jpg
    IMG_20230825_122853.jpg
    2.7 MB · Views: 3
  • IMG_20230825_122850.jpg
    IMG_20230825_122850.jpg
    2.8 MB · Views: 3
  • IMG_20230825_115200.jpg
    IMG_20230825_115200.jpg
    2.2 MB · Views: 3
  • IMG_20230825_115149.jpg
    IMG_20230825_115149.jpg
    3.2 MB · Views: 3
  • IMG_20230824_131223.jpg
    IMG_20230824_131223.jpg
    4.8 MB · Views: 3
Last edited:
Now that you mention it, it did have a warning triangle on the back and a tow strap on the front :!:
Tow mode also wasn't engaged, so that could definitely have done it.
The guy lives about 10 miles from the workshop, so lots of time to cook it.
 
Looks like it grenaded from overspeed, rather than melting, then all the bits ground each other up really thoroughly...best bet is during the towing--probably was towed at high road speed or even freeway speed, without disconnecting the motor from the wheels, so failure probably occurred shortly after starting out then kept destroying itself the rest of the trip.

Seen a few like that in various conversion threads over the years, mostly on DIYElectricCar forums, often enough from being towed or coasting downhill (but still in-gear) faster than "max design speed".... :(
 