I see what you mean. According to the chart 0.15 x 8 is only equivalent to 7g wire. 0.3 is like 14g. 14g seems small for 20 amps? Maybe use 0.3 with 0.15 welded on top?This depends on your pack layout. Perhaps you can draw it, or at least describe it? I just skimmed through the thread quickly, so perhaps you've stated it and I just missed it, but it seems like you're planning a 100a capable pack. Meaning your total series connections need to be able to handle 100a. How many strips of nickel will be in the parallel connections? I couldn't tell for sure from your descriptions in the above posts whether you're planning 7p or 10p.
Nickel Strip ratings
Hi All, I am just wondering if someone can point me to a chart or resource that will show me the current ratings for this: https://eu.nkon.nl/accessories/battery-solder-strip/nikkel-batterijpack-verbinding-soldeerstrip-27mm.html nickel strip 27mm x 0.15m. I have asked Nkon and they don't...endless-sphere.com
If you follow this chart, you'll see that .15x8mm nickel is only good for about 5 amps. To safely carry 100a, you'd need 20. If you're planning 10p, and there's 10 series connection points between all your parallel groups, then it's "possible" to get what you need by stacking 2ea .15x8mm strips per nickel connection. If you're doing 7p, I wouldn't recommend stacking 3 strips.
I'm finally starting to understand how, and why, to build a pack with more parallel cell groups as opposed to all series cell groups. Apparently building with parallel cell groups in series, instead of single cell groups in parallel you get less sag. I hadn't thought about that before, but it makes sense to me. If I'm wrong about this feel free to say so. Nothing is set in stone.I believe that the ideal layout for a battery to stack each group in one column. Then place the groups end to end, so that the series current flows directly from one cell to the next. Here is how it would look for a 13S-7P. Each horizontal section of nickel needs to be thick enough to carry 1/7 of the battery current, The vertical connects are only for small parallel currents, so don't have to be very heavy, At the positive and negative ends of the array, you have to connect the power cables so the current flows evenly out of all 7 cells.
View attachment 351829
I do not like stacking strips, I think they can be problematic when you do more than two. However, you have a big welder so it shouldn't be a problem.
The bare minimum is 800 A for proper functioning. 1200 to 2000 A is the recommended range. 496 A is inadequate. That battery is very tired.What makes me suspicious of the battery is when I get to the last calibration step, I short the probes, hit the button, and the first thing on the display is, under current, then it scrolls through 4 items. R 2.89, STD 46.0, I 496a, T 28.9c
Thank you very much for the reply. That's very reassuring, I was going to try a new battery next.The bare minimum is 800 A for proper functioning. 1200 to 2000 A is the recommended range. 496 A is inadequate. That battery is very tired.
Your phrasing may be confusing ... perhaps why no others have replied to above quote.It may have been less confusing as ...I'm finally starting to understand how, and why, to build a pack with more parallel cell groups as opposed to all series cell groups. Apparently building with parallel cell groups in series, instead of single cell groups in parallel you get less sag. I hadn't thought about that before, but it makes sense to me. If I'm wrong about this feel free to say so. Nothing is set in stone.
"I'm now thinking in terms of 20 cells in each series "string" with 7 cells in each parallel "group" (20s7p) for a total of 20 such parallel groups of 7p. That still ends up 72v (nominal cell voltage of 3.6V)".I'm now thinking in terms of 20 groups of 7 parallel cells each. That still ends up 72v and 140 cells.
This has always been a question in my mind. After having the bms in my hand and seeing how it's wired, now I understand.BMS doesn't have a "P" number, only S, because all cells in P are already connected together and thus use the same balance/sense wire from the BMS.
Thank you for sharing your experience. I like the idea of not having to fold the halves together, and I was already looking into finding some H pattern nickel.I wouldn't fold a stack of 35 cells on top of another. It's hard to spot weld them and fold them straight, and you have to adjust the strips to fit an insulator between the top and bottom. I've done it, and I get crooked stacks. If I have to stack them now, I would extend separate strips of nickel from each half, and solder them together later.
If you can get the H-pattern in pure nickel, you get both parallel and series at the same time.
You are going to have three long strips where you have to bolster the nickel. The first two are the positive and negative ends where 7 cells have to flow into B+ and B-. The third will be between groups 10 and 11 where 14 cells in a row are connected. In my opinion, making it carry 40A is tough enough, and you want 100A? Figure on adding a lot of copper wire.