ichiban said:The double plating with copper and nickel will be by industrial process, easily control with accurate result.
1st plating with copper 0.075mm thick is automatic on both side, front and back with same thickness.
2nd plating with nickel 0.025mm thick is likewise.
Total of 0.3mm thick strip with 0.15mm copper layer thick (0.075mm x 2).
Any comments ? Will this be good for kWeld ?
Look into CuNi18Zn20 (Copper Nickel Zinc Alloy) for connecting strips or plates for battery building. Timo Hoyer from Germany uses it.
https://www.facebook.com/timucin.hoyer