Valy,
Thanks for the aluminum polishing lesson. Look at my 2 inch aluminum mail box post. Pictures are not so good. Would like to see [pictures of camera's for taking pictures of Tools for Bike Builders]
View attachment pipe01.jpg
View attachment 2
Pipe is just practice for my next aluminum polishing project. See pictures of 2006 Morgan Olson 11 foot Step Van.
http://06stepvan.com/
View attachment 1
As to the debate of how to best protect polished aluminum? I say NO coatings. Using this stuff along with prayer to prevent corrosion of aluminum.
http://triple-s.com/
METAL CLEANER & POLISH #05013
A blend of special cleaners and polish oils
specifically designed for use on stainless
steel and other metal surfaces.
• Oil-based cleaner/polish
• Cleans, protects & polishes
• Leaves an ultra high gloss film
• Pleasant lemon fragrance