papasapien said:
also what will the difference be if i use 63/37 vs 60/40? is that better recommended for electrical reasons or just solder preference?
No practical difference either way. The performance of the flux in the core will make more difference than the alloy.
Lead free? That's another matter, and something to steer clear of.